PENGARUH PENGERJAAN AKHIR TERHADAP STABILITAS DIMENSI KAYU

Main Author: Balfas, Jamal
Other Authors: Pusat Penelitian dan Pengembangan Hasil Hutan
Format: Article info application/pdf eJournal
Bahasa: ind
Terbitan: Pusat Penelitian dan Pengembangan Hasil Hutan , 2017
Subjects:
Online Access: http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603
http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603/4209
ctrlnum --ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3603
fullrecord <?xml version="1.0"?> <dc schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd"><title lang="id-ID">PENGARUH PENGERJAAN AKHIR TERHADAP STABILITAS DIMENSI KAYU</title><creator>Balfas, Jamal</creator><subject lang="id-ID">Stabilitas; dimensi kayu; pengerjaan akhir</subject><description lang="id-ID">This study was designed to determine the ability of six commercial exterior finishes (2 clear coats and 4 opaque coats) in protecting wood from dimensional changes. Two wood species, jabon (Anthocephalus cadamba Miq.) and mangium (Acacia mangium Willd.) were used in this study. Samples were seasoned to air-dry condition (moisture content of 15-17%) and then divided into groups on the basis of treatments and grain orientation (radial and tangential). Application of each exterior finish was undertaken according to procedures suggested by the finish manufacturer. The effectiveness of treatments to dimensionally stabilize wood was determined by measurements of wood swelling within 72-hours immersion and calculation of anti-swelling efficiency (ASE). Results of observations made to this stage showed that the effect of finishing on wood dimensional stability varied according to wood species, grain orientation and type offinish coat. Finishing had a greater dimensional stabilizing effect on jabon than mangium. Reduction of swelling due to finishing was greater in tangential compared to radial boards. The use of clear coats significantly gave less protection on wood stability than that of opaque coats. Anti-swelling efficiency of all treatments markedly decreased with increasing period of immersion.</description><publisher lang="id-ID">Pusat Penelitian dan Pengembangan Hasil Hutan</publisher><contributor lang="id-ID">Pusat Penelitian dan Pengembangan Hasil Hutan</contributor><date>2017-08-23</date><type>Journal:Article</type><type>Other:info:eu-repo/semantics/publishedVersion</type><type>Other:</type><type>Other:</type><type>File:application/pdf</type><identifier>http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603</identifier><identifier>10.20886/jphh.1994.12.2.77-83</identifier><source lang="en-US">Jurnal Penelitian Hasil Hutan; Vol 12, No 2 (1994): Jurnal Penelitian Hasil Hutan; 70-75</source><source lang="id-ID">Jurnal Penelitian Hasil Hutan; Vol 12, No 2 (1994): Jurnal Penelitian Hasil Hutan; 70-75</source><source>2442-8957</source><source>0216-4329</source><language>ind</language><relation>http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603/4209</relation><rights lang="en-US">Copyright (c) 2017 Jurnal Penelitian Hasil Hutan</rights><rights lang="en-US">http://creativecommons.org/licenses/by-nc-sa/4.0</rights><recordID>--ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3603</recordID></dc>
language ind
format Journal:Article
Journal
Other:info:eu-repo/semantics/publishedVersion
Other
Other:
File:application/pdf
File
Journal:eJournal
author Balfas, Jamal
author2 Pusat Penelitian dan Pengembangan Hasil Hutan
title PENGARUH PENGERJAAN AKHIR TERHADAP STABILITAS DIMENSI KAYU
publisher Pusat Penelitian dan Pengembangan Hasil Hutan
publishDate 2017
topic Stabilitas
dimensi kayu
pengerjaan akhir
url http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603
http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3603/4209
contents This study was designed to determine the ability of six commercial exterior finishes (2 clear coats and 4 opaque coats) in protecting wood from dimensional changes. Two wood species, jabon (Anthocephalus cadamba Miq.) and mangium (Acacia mangium Willd.) were used in this study. Samples were seasoned to air-dry condition (moisture content of 15-17%) and then divided into groups on the basis of treatments and grain orientation (radial and tangential). Application of each exterior finish was undertaken according to procedures suggested by the finish manufacturer. The effectiveness of treatments to dimensionally stabilize wood was determined by measurements of wood swelling within 72-hours immersion and calculation of anti-swelling efficiency (ASE). Results of observations made to this stage showed that the effect of finishing on wood dimensional stability varied according to wood species, grain orientation and type offinish coat. Finishing had a greater dimensional stabilizing effect on jabon than mangium. Reduction of swelling due to finishing was greater in tangential compared to radial boards. The use of clear coats significantly gave less protection on wood stability than that of opaque coats. Anti-swelling efficiency of all treatments markedly decreased with increasing period of immersion.
id IOS3429.--ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3603
institution Kementerian Lingkungan Hidup dan Kehutanan Republik Indonesia
institution_id 475
institution_type library:special
library
library Perpustakaan Kementerian Lingkungan Hidup dan Kehutanan RI
library_id 121
collection Indonesian Journal of Forestry Research
repository_id 3429
subject_area Kehutanan
Lingkungan
Pertanian
city BOGOR
province JAWA BARAT
repoId IOS3429
first_indexed 2018-04-01T02:21:39Z
last_indexed 2019-05-06T00:33:08Z
recordtype dc
merged_child_boolean 1
_version_ 1800763743223676928
score 17.538404