SIFAT VENIR DAN KAYU LAPIS 7 JENIS KAYU DARI MALUKU

Main Authors: Iskandar, M I, Kliwon, Suwandi, Sutigno, Paribotro
Other Authors: Pusat Litbang Hasil Hutan
Format: Article info application/pdf eJournal
Bahasa: ind
Terbitan: Pusat Penelitian dan Pengembangan Hasil Hutan , 2017
Online Access: http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209
http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209/2524
ctrlnum --ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3209
fullrecord <?xml version="1.0"?> <dc schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd"><title lang="id-ID">SIFAT VENIR DAN KAYU LAPIS 7 JENIS KAYU DARI MALUKU</title><creator>Iskandar, M I</creator><creator>Kliwon, Suwandi</creator><creator>Sutigno, Paribotro</creator><subject lang="id-ID"/><description lang="id-ID">&#xA0;The characteristics studied&#xA0; are peeling properties,&#xA0; physical&#xA0; properties&#xA0; of&#xA0; the veneer, gluing properties&#xA0; and some physical&#xA0; and&#xA0; mechanical properties&#xA0; of&#xA0; the plywood&#xA0;&#xA0; (both&#xA0; triplex and multiplex).All logs from the 7 wood species could be peeled satisfactorily&#xA0; in cold condition.&#xA0;&#xA0; Veneer of &#xA0;0.9 mm and 1.5&#xA0; mm thickness&#xA0; could be produced at a cutting&#xA0; angle between&#xA0; 91&#xB0;-93&#xB0;.Average shrinkage&#xA0; of&#xA0; the veneer is 7%.&#xA0; Average swelling from oven dry condition&#xA0; is 3%.Water resistant,&#xA0; bonding&#xA0; strength&#xA0; for all wood&#xA0; species studied&#xA0; meet Indonesian,&#xA0;&#xA0; Japanese&#xA0; and German standards. Average thickness reduction due to pressing in the plywood&#xA0;&#xA0; manufacturing&#xA0; process&#xA0; is 0.15 mm.Specific&#xA0; gravity&#xA0; of&#xA0; the plywood&#xA0;&#xA0; is about&#xA0; 6 percent&#xA0; higher than that&#xA0; of&#xA0; the wood from&#xA0;&#xA0; which it is made&#xA0; of</description><publisher lang="id-ID">Pusat Penelitian dan Pengembangan Hasil Hutan</publisher><contributor lang="id-ID">Pusat Litbang Hasil Hutan</contributor><date>2017-08-15</date><type>Journal:Article</type><type>Other:info:eu-repo/semantics/publishedVersion</type><type>Other:</type><type>Other:</type><type>File:application/pdf</type><identifier>http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209</identifier><identifier>10.20886/jphh.1987.4.2.36-41</identifier><source lang="en-US">Jurnal Penelitian Hasil Hutan; Vol 4, No 2 (1987): Jurnal Penelitian Hasil Hutan; 36-41</source><source lang="id-ID">Jurnal Penelitian Hasil Hutan; Vol 4, No 2 (1987): Jurnal Penelitian Hasil Hutan; 36-41</source><source>2442-8957</source><source>0216-4329</source><language>ind</language><relation>http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209/2524</relation><rights lang="en-US">Copyright (c) 1987 Jurnal Penelitian Hasil Hutan</rights><rights lang="en-US">http://creativecommons.org/licenses/by-nc-sa/4.0</rights><recordID>--ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3209</recordID></dc>
language ind
format Journal:Article
Journal
Other:info:eu-repo/semantics/publishedVersion
Other
Other:
File:application/pdf
File
Journal:eJournal
author Iskandar, M I
Kliwon, Suwandi
Sutigno, Paribotro
author2 Pusat Litbang Hasil Hutan
title SIFAT VENIR DAN KAYU LAPIS 7 JENIS KAYU DARI MALUKU
publisher Pusat Penelitian dan Pengembangan Hasil Hutan
publishDate 2017
url http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209
http://ejournal.forda-mof.org/ejournal-litbang/index.php/JPHH/article/view/3209/2524
contents The characteristics studied are peeling properties, physical properties of the veneer, gluing properties and some physical and mechanical properties of the plywood (both triplex and multiplex).All logs from the 7 wood species could be peeled satisfactorily in cold condition. Veneer of 0.9 mm and 1.5 mm thickness could be produced at a cutting angle between 91°-93°.Average shrinkage of the veneer is 7%. Average swelling from oven dry condition is 3%.Water resistant, bonding strength for all wood species studied meet Indonesian, Japanese and German standards. Average thickness reduction due to pressing in the plywood manufacturing process is 0.15 mm.Specific gravity of the plywood is about 6 percent higher than that of the wood from which it is made of
id IOS3429.--ejournal.forda-mof.org-ejournal-litbang-index.php-index-oai?verb=ListSets:article-3209
institution Kementerian Lingkungan Hidup dan Kehutanan Republik Indonesia
institution_id 475
institution_type library:special
library
library Perpustakaan Kementerian Lingkungan Hidup dan Kehutanan RI
library_id 121
collection Indonesian Journal of Forestry Research
repository_id 3429
subject_area Kehutanan
Lingkungan
Pertanian
city BOGOR
province JAWA BARAT
repoId IOS3429
first_indexed 2019-05-06T00:35:36Z
last_indexed 2019-05-06T00:35:36Z
recordtype dc
merged_child_boolean 1
_version_ 1800763746815049728
score 17.538404