  • The Brønsted acid site was determined by using volumetric and Potentiometrie titration method. The result showed that the Brønsted acid sites of synthesized aluminosilicate using volumetric titration method are aluminosilicate-1: 0.5491; aluminosilicate-2: 0.5523; and aluminosilicate-3: 0.5772 mmol/g and using potentiometric titration method are aluminosilicate-1: 4.7087; aluminosilicate-2: 5.5739; and aluminosilicate-3: 8.1059 mmol/g. FTIR-pyridine also showed the same trend line, the Brønsted acid sites concentration increased by the increasing of Si/Al mole ratio. The results of the measurement using FTIR-pyridine showed the Brønsted acid sites concentration of aluminosilicate-1; aluminosilicate-2; and aluminosilicate-3 were 0.0293; 0.330; and 0.0336 mmol/g, respectively. The Brønsted acid sites concentration of aluminosilicate was higher using volumetric titration and potentiometric titration methods than using the FTIR-pyridine method, but the trend line was the same, the higher Si/Al mole ratio, concentration of Brønsted acid sites increased.